Dear Experts,

Need your expert advise on below :

Background :
Equipment data sheet specifies HIC resistant material to be used.
And applicable EIL specification 6-79-0013 R1 (Material requirements for Carbon steel components used in Sour service for petroleum refinery environment)
I understand these specification calls for HIC testing of Plates & Rolled products(pipes fittings made from plates) only.

Question :
Does EIL Specification 6-79-0013 R1 calls for HIC testing of components other than plates & rolled products such as Forgings, pipes, fittings, fasteners as well?

Kindly confirm with clarifications for better understanding.


Best Regards, 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiDOxk%3DNOyKmTeY%3DdPa1WTvc%2Bw51q0M1AbsANrqFL5fXwzPhg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...