Re: [MW:30516] Re: Impact Test

YES, PQR QUALIFICATION WITH IMPACT TEST IS TO BE CARRIED OUT FOR SAFE SIDE. 
Regards

Lalit Vadadoriya
Dy.Manager(Piping)
Engineers India Limited

Mob.9377072930


On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AMkqLQr%2BV0KXTtf%3DG%2BX03SpPg8z92ePJqHXO0PJpZctg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKjb_1LhrQxE7es2Bx6tYyyh8j-BnUFO8TKbrrWjeBxuC1Ca5w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...