[MW:30483] Filler grouping as per API 1104

Dear experts,

I have a PQR qualified for branch welding as per API 1104.  Low hydrogen elcerodes (ER 70S2 and E7018-1) were used for branch welding as specifications calls for it.
Now can I develop a WPS  using ER70s2 and E7018? 
I am unclear with the clause 5.4.2.6 b) in API 1104. 

Kindly advise 

Thanks and regards
TDK Yokesh 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuoNfQWovuqnBCd36k0PioOH0eAE-SRYQrLXTMo1o_BStA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...