Dear

Where is written that after welding immediate do PWHT. 
you can do PWHT after one, two or more days. 
We r doing preheat during welding and after welding complete, we have continue preheat and come down temp upto ATM. 

Regards 
A p gupta 


On Fri, 8 Nov 2019 at 8:49, PARAI Reaction Channel
<saravanshyla@gmail.com> wrote:
Dear Experts,

For one of our project, 

With reference to the sketch shown below, we are going to weld 4 number of Single V Butt joints for A335P11 to itself ( P No. 4 ), pipe Thk of max 28.6 mm by using GTAW & FCAW process ,

Preheat Tempr. of Min. 120 Deg C ( Plan to use Burner ) and PWHT from 650 to 707 Deg C as per ASME B31.3 code.

After we complete the welding in our shop and bring back to the normal ambient tempr. around 15 Deg C, can we do PWHT after 1 or 2 days gap and then we do RT and PT ?

I worry that, during winter in Korea, the ambient tempr. may drop to Minus 10 Deg C.

As there is no weld spec from client for P No.4 , can we do PWHT after 2 days gap.

Please suggest me with any weld instructions for P. No.4 , Preheat maintenance, in order to avoid any crack after welding and with delayed PWHT condition.

image.png

With best regards,
Saravanan.Sornam,
Korea

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkKyaKN%2BXoGTzSC7ok%3DnYVeUwbp1CYp-YyEJn2CYFrvebg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2041700894.1080110.1573185305327%40mail.yahoo.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...