Tuesday, July 9, 2019

Re: [MW:29802] ER70S-2 and ER70S-6 (GTAW Process)

ER70S-6 chemical composition does not allow A-No allocation. 

Στις Πέμ, 6 Ιουν 2019, 14:40 ο χρήστης Revdiwala Darshan <darshanmrevdiwala@gmail.com> έγραψε:
Please refer QW-404.12 (f) for code restriction.

Regards,
Darshan

On Mon, 3 Jun 2019, 6:26 pm Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Code doesn't restrict but u will not get it in cut to length. Hardness will also increase due to more Mn, Si. It is better to add ER 70S3

On Mon, 3 Jun 2019 7:48 pm K K, <karan.hbl@gmail.com> wrote:
Dear All,

My PQR is qualified with ER70S-2.

Can I use ( Mention) ER70S-6 in WPS.

Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/76403448-7204-4bda-83fd-21deebafcaa5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO5SQ98yk8ZEshkBi4OXaboJN106ZjbFnzTQrnSPrNsqw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABDq6ggVhFeygjQ-jUJy%3DDTczBW5D-wk3KXjNohjDMnHmHVjhw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40COLfUzYWJtNBMJVb%3DHGU1-t1fykQEzUGSDU5%3Du-sfr7A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...