Dear experts,
Please clarify for impact test requirements of below variables.
Construction code ASME B31.3
Material A106 Gr. B
The thickness of Pipe. 17.48 mm
Temperature Limit 0^ F (-17.78^ C)
PWHT yes.
Table A-1 refers to curve B
Table 323.2.2A minimum Temperature without Impact Testing for CS showing under curve B 9^ F ( 12.8^ C).
My Question is for above case Impact testing for WPS qualification is required?
Please clarify for impact test requirements of below variables.
Construction code ASME B31.3
Material A106 Gr. B
The thickness of Pipe. 17.48 mm
Temperature Limit 0^ F (-17.78^ C)
PWHT yes.
Table A-1 refers to curve B
Table 323.2.2A minimum Temperature without Impact Testing for CS showing under curve B 9^ F ( 12.8^ C).
My Question is for above case Impact testing for WPS qualification is required?
Regards,
Muhammad Babur Khan Lashari
Sr. QA/QC Inspector (Welding)
(CSWIP 3.1 / CWI II From PWI)
Mob: + 966 58 2774568 / 050 5193275
PAK : + 92 334 6186285 (Whatsapp)
Skype: babur.lashari
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN53wK1Vs8CgXP0uzAFyPAUNQ-gbaeg7axU9zRQZsXhV9p19jg%40mail.gmail.com.
Comments