In my opinion, only bend tests as stipulated in QW -452 of ASME Section 09 is applicable.  

 

And the interpretation is as below,

In ASME B31.3 Chapter 09, the requirements are as below

1.       K328.2.1 Qualification Requirements.

           e) Mechanical testing is required for all performance

qualification tests.

 

And if we refer to ASME Section 09, QW-302 TYPE OF TEST REQUIRED, QW-302.1 Mechanical Tests which in turn reference to QW-452. 

Thus, only bend test is considered as mechanical testing for welder qualification tests.

 

Regards,

Sudhakar K

Welding Engineer 




On Sun, Jul 21, 2019 at 8:05 AM Kataiah Pamula <pkataiah@gmail.com> wrote:
Dear Experts,

As per ASME B31.3  Chapter IX Welding, does performance qualification requires all mechanical testing to do be done including tensile, bend, impact, lateral expansion to be measured apart form RT.

As per Clause K328.2.1(e)

(e) Mechanical testing is required for all performance
qualification tests.

Pl share your valuable inputs.

best regards

Kataiah



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFM%2B2hzyD_p1qtymWBGz%2BcnBdN%3Djqj7ms0tejXDKvG0uQU2ryA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfZfcM0%2B%3DRw1nXdCrAKp7Pae0oX8f0boH%3Dn7Wc0Q%2BAc%2BZth_g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...