No, you cannot, base metal thickness and deposited weld metal thickness are two different essential variables

Στις Τετ, 17 Ιουλ 2019 στις 6:19 π.μ., ο/η Isac Passaura <isac.passaura@gmail.com> έγραψε:
Dear Experts,

I have some difficulty to interpret the requirements of ASME section IX

I have a  PQR Based on a dual process GTAW+SMAW ( 8 mm+17,4 mm) on an 25,4 mm butt weld.

Can I make a weld using only the GTAW process, base metal with a thickness of less than 5mm?

Are the image conditions correct?



Please give with details explanation regarding my above difficulty.


Thanks and Regards


Isac







--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c74dd763-9499-4097-b2cc-5cd52a84818d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AsQSYJbNVBh-O7xWCdc_ReqPJ%3DmjZr3wOx_V9aGtoZGA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...