Wednesday, July 31, 2019

Re: [MW:29902] Re: PWHT THICKNESS

Hi,
ASME Section VIII Div.1 for pressure vessel construction. In your case its a base frame (not pressure vessel) so the construction code will be AWS D1.1. As per AWS D1.1, If heat treatment required by your contract or PO documents/project specification then  you should do as per AWS D1.1, Section 5.8.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Tuesday, July 30, 2019, 10:38:56 PM GMT+7, Sumit Baliram Bhadakwad <bhadakwad.sumit@gmail.com> wrote:


Hello Sir ,

We are following ASME SECTION VIII DIV 1. Please guide me.
Actually I am confused between UCS-56(d)(1) through (5) term "maximum material thickness " & UW-40(f)(1) through (6).

I want to  below details .

unrestricted heating rate up to .
Heating rate of maximum :- 
Holding temperature 
Soaking Time : 
Cooling rate of maximum:- 
Unrestricted cooling rate -

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/6103e818-5fad-4e83-b523-320abcca3bbf%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...