Friday, July 19, 2019

RE: [SOCIAL NETWORK] [MW:29877] Difference between the Grades

Shri Manoj Parabhakaran

 

Ye, basically for strength and the related changes in the elongation, chemical composition etc

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Manoj Prabakaran.M
Sent: 19 July 2019 11:16
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [SOCIAL NETWORK] [MW:29875] Difference between the Grades

 

Dear Experts,

 

I wish to know that, What is the exact difference in SA 516 Gr.50, Gr.60 and Gr.70.

 

As we all know that major difference is strength, if anything else?

 

If Gr.50 and Gr.60 are manufacturing by SAIL/JINDAL?

 

Please let me know and do the needful.

 

Regads,

Manoj Prabakaran.M 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95bf9829-8dd8-4a55-b633-07d50b1b3313%40googlegroups.com.

---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately. Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences. While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail. ---------------------------------------------------------------------------------------------------------

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...