Dear All,

I have query about PWHT,

I have qualified WPS and PQR, as per B31.3.(But our requirements as per B31.3 and B31.1 )

Can you please tell me some one, what is difference between theses both standard for PWHT.  

( As per my knowledge  1) PWHT temperature for ASME P number 04 material is different from ASME B31.3 (process) : range 704-746°C to ASME B31.1 (Power) : range 650-700°C.)

Below I have given some WPS parameters for PWHT, please clarify me whether the parameters are correct or Not. 

According to B31.3 -

Material : ASTM A 335 P11 to ASTM A 335 P11 - ( PNo-4; G.No-1 to PNo-4; G.No-1 )
Process : GTAW
Test coupon Thickness :  19.05 mm
PWHT- Temp range - 690°C- 705°C
Heating range : 200°C/hr
Cooling range : 200°C/hr
Interpass temp : 315°C
Post Heating : 300°C -350°C ; holding thickness 10mm to 20mm -30 min / 20mm to 30mm - 90min.

And regarding Backing -  PQR is qualified with Argon, can we use Nitrogen in WPS.

Experts i am looking your favorable reply on my query.

Thanks

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/270bf5d4-65f6-4e9c-bea5-331611e4edfe%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...