Dear Mr. Venkat. G
-- Thanks for your support and i would like to be inform if selected electrode meet NACE MR-0175 and hardness limited to 23 Max HRC
during my search i found E8018-B2 or E8018-C3 more accurate for H2S or Sure Service.
**Last question if i can use this electrode for Root or i have to select another electrode for pipe Root.
On Wednesday, June 12, 2019 at 6:55:51 PM UTC+3, Venkat QMR (IRCA, Lead Auditor)) wrote:
On Wednesday, June 12, 2019 at 6:55:51 PM UTC+3, Venkat QMR (IRCA, Lead Auditor)) wrote:
Hi Ehab,
- E 10018-D2 - Electrode - SMAW
- ER 80S-D2 - FIller Wire - GTAW
You can use for SMAW first one.Best Regards,Venkat. GOn Wed, Jun 12, 2019 at 8:22 AM Ehab Ahmed <elpop...@gmail.com> wrote:--Dear Sirs,Pleas help me to Select electrode ? for AISI 4130 (70-75 Ksi) and API 5CT L80 Pipe materials to weld by SMAW.Using ASME IX Code.Thanks and Best Regards,Ehab Ahmed
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .20385728-b6dc-46fa-b65c- 7fc06c8a7b47%40googlegroups. com
For more options, visit https://groups.google.com/d/optout .
--Venkatachalam GovindanQHSE Lead / Trainer(IRCA Registered Lead Auditor & API / CQI Practitioner)+965 97604989, +919840502376 (WhatsApp only)
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e1394032-53d1-4d9d-976c-880537c6f1a0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments