Re: [MW:29849] Asme Section IX Thickness range qualification

Yes you can, 

Your 25.4 mm with gtaw and smaw can write 2t ranges from your PQR for what has been deposited individually.

you are going to write a WPS or below snap is ready WPS?

Check impact / PWHT requirements for what you qualified and what recommended in production joint.

Thanks.
Mohamed Muneeb Mahaboob.
 
Date: 2019-07-17 04:25
Subject: [MW:29843] Asme Section IX Thickness range qualification
Dear Experts,

I have some difficulty to interpret the requirements of ASME section IX

I have a  PQR Based on a dual process GTAW+SMAW ( 8 mm+17,4 mm) on an 25,4 mm butt weld.

Can I make a weld using only the GTAW process, base metal with a thickness of less than 5mm?

Are the image conditions correct?



Please give with details explanation regarding my above difficulty.


Thanks and Regards


Isac







--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c74dd763-9499-4097-b2cc-5cd52a84818d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...