On Wednesday, June 12, 2019 at 8:22:55 AM UTC+3, Ehab Ahmed wrote:
Dear Sirs,Pleas help me to Select electrode ? for AISI 4130 (70-75 Ksi) and API 5CT L80 Pipe materials to weld by SMAW.Using ASME IX Code. PQR should Meet Requirement according to NACE MR0175
Thanks and Best Regards,Ehab Ahmed