Re: [MW:25775] reg: Maximum interpass temperature in a WPS

As far as non essential variable is concern and impact is not required interpass is ok but if client have some requirement mention in their specifications then that should be followed and as thk range 1.5 to 14.22 mm is concerned interpass can be 150 degree also.

Regards,
Mohit Aggarwal.


On Nov 29, 2016 8:04 AM, "Prince C thomas" <princecthomas@gmail.com> wrote:
Dear Sir's,

Kindly reply to  my below query:

We have project approved WPS with following details:

Material Spec: ASTM A106 Gr.B

P no:1/Group no:1

Material thickness: 1.5 -14.22 mm

Welding process: GTAW+SMAW

GTAW-Filler wire : ER 70S-2

SMAW-Electrode: E 7018

Preheat - 10 deg minimum

Interpass temp: 200 Deg C Maximum

In the PQR: pre heat temperature:38 deg C

                  Interpass temperature: 68 deg C maximum



Since interpass temperature is not a essential variable (Impact test is not applicable); but still our client is asking to recheck the max.interpass temperature value ( 200 Deg C) in the WPS. How to convince client to get approval on the same?






--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb942dff-ef50-4ad8-bd7c-a62ed99ac06b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPMWYj4MosAoVoa5hdWef8jPtZ%3Dsdguvcp%3DUfyVub5kUtQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...