I am looking for some data on operating factor for FCAW - that is the ratio between a theoretical deposition rate with 1.2mm FCAW and actual production relevant to a fabrication shop or site welding structural steel in thicknesses between 20mm and 60mm. Some work is in fabrication shops and some is in the yard. Would 40% be constantly achievable, ignoring time for meal breaks and repairs? That is the sort of figure stated in recommendations from consumable suppliers.
All or any information would be welcome.
Alan Denney