Dear Sir,
If we have PQR with PWHT for T-T 610°C & 3 Hrs. for Thickness 40mm as per ASME Sec. IX. for SMAW. Consequently we have WPS for Range of 5 to 200mm Thickness (PQR is tested for Impact at -27°C).
Now the Confusion is can we use same PQR to Prepare WPS for 25mm thick Production weld with T-T 610°C & 1Hrs if supplementary essentials are applicable? Now as per Table QW253 & QW 407.2 the production weld PWHT T-T cycle essentially Equivalent or at least 80%.
QW-407.2 A change in the postweld heat treatment
(see QW-407.1) temperature and time range
The procedure qualification test shall be subjected to
PWHT essentially equivalent to that encountered in the
fabrication of production welds, including at least 80%
of the aggregate times at temperature(s). The PWHT total
time(s) at temperature(s) may be applied in one heating
cycle.
Bhavesh
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABACBz0DASBbzj-9NckzknVmQ5b2xLQxBxyYJxTZ-TeJho6Btg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments