Hi,
It is either 6013 or 7018 - whatever it may be, you have to establish a WPS and then qualify the PQR -
If all the particulars (mechanical, chemical and etc.) are complying to the specifications and to client requirements in the established PQR - then there will not be any issue of using any consumable.
Or...
If your client specification has called for any specific requirement of the electrode (say E 7018) then u have to qualify the PQR with that only.
Or...
If you have any constrain in using any electrode (practical problem, approach, easiness in welding, weld metal deposition rates, any power source limitations, any specific NDT requirement and many more particulars) then also, you may opt for 7018 or any other grade to suit requirement -
But in and overall - you have to qualify the PQR with all the variables...
Hope u understand...
Thanks & Regards,
Lakshman Kumar B,
Project Manager.
Navayuga Engineering Company LTD
Corp Off: Plot no 379, Road No 10,
Jubileehills, Hyderabad.500033 India.
Tel - +91 -40-2333 9990/91/92 – Ext 398
Fax: +91-40-2333 7789
Mob - +91 9440031459.
Email –lakshmankumarb@navayuga.com
http://www.necltd.com/
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Prasad Rode
Sent: Wednesday, November 30, 2016 1:23 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25779] Limits of E6013 in pressure vessel (sec viii div 1)
Dear sir,
In fabrication of pressure vessel from 10mm thk plate, would we allow to use E6013 electrode.
Is any where given in code of sec viii div 1, about limits of E6013, or only E7018 is allow.
Regards
Prasad Rode
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4e2ec747-1d48-40dd-a8de-522e133423bd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00ff01d24afd%24c43eff90%244cbcfeb0%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment