which grades of structural steel are you going to use?
If 6013 is matching the properties of the involved structural steel and the welders have no experience with basic electrodes handling, then better go with 6013

2016-11-14 12:38 GMT+02:00 Brajendra Patel <brajendra.patel@koso.co.in>:

Dear Anil,

 

E6013 is best suited for structural weld, but for better quality you can  use E7018 with proper baking.

 

Regards,

Brajendra Patel

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anil Kumar
Sent: Monday, November 14, 2016 3:51 PM
To: Materials & Welding
Subject: [MW:25691] which electrode to be used for structural welding 6013 or 7018

 

Hi,

 

      for structural welding which electrode will be used 6013 or 7018. following code is AWSD1.1

 

 

 

 

Thanks & Regards

Anil Kumar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55fe6399-95fa-4fe9-ae42-25e8eea67ead%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D288AF0A8981664D8CC97F6CFF20756B38856540%40XCELLMBX01.xcellinfra.india.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AbN5cXe-mrD84qJ%2B6DToyKaOATc%2BR84-1NW%2BoMW%3DVgKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...