My experience is that it does not work,  and this is not surprising. I have had eddy current testing used over painted surfaces to detect underlying cracks with good results, in that cracks were reliably detected. You would need to trial it with coatings on the calibration block.

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george keribo
Sent: 18 November 2016 12:48
To: materials-welding@googlegroups.com
Subject: [MW:25727] MPI on painted joint

 

Please I wanted to know any code reference for painted surface magnetic particle test

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4Ss47uNCqgDQUGh0%2BpLM40NH8wqJiP4aaDsWxio_mWqHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...