Dear Sridhar,

Here we are talking about Pre-Qualified WPS i.e..pWPS.
To initiate the welding, pWPS required.

On Tuesday, November 15, 2016 at 9:09:41 AM UTC+5:30, sridhar wrote:
It means if you have already qualified a procedure for similar P nos, 
say, as per ASME sec IX  or any code, you can refer it in your new 
WPS if done with AWS D 1.1 for same P nos. No need to do a PQR 
for the new WPS.

Sridhar.



From: pankaj phuse <pankaj...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Monday, 14 November 2016 10:41 AM
Subject: [MW:25687] Re: what is pre qualified WPS as per AWS D1.1

Prequalified welding procedure specification includes a weld joint specified in a governing code that does not require validation of welding parameters through the performance of a procedure qualification test. So, a prequalified WPS does not need a supporting Procedure Qualification test Record (PQR).

Regards
Pankaj Phuse
Welding Engineer
CSWIP 3.1

On Sunday, November 13, 2016 at 7:00:56 PM UTC+5:30, Anil Kumar wrote:
Other recipients:
Dear All What is pre qualified WPS as per AWS D1.1 Its allows to write a WPS without PQR...? Please explain Regards Samshuddin.K
Dear All

What is pre qualified WPS as per AWS D1.1

Its allows to write a WPS without PQR...?

Please explain
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/035b3dca-c195-40db-b4e4-ac04f2d0e618%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5827c8e3-c316-40d2-a967-4a55eeef7cf5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...