[MW:25701] thickness on painted vessel

Dear Experts,

Greetings.

Just expecting your views for the UT- thickness measurements on a
painted pressure vessel (shell thick 54 mm & head 65mm) painting
thickness -250 microns. material SA 516 Gr. 70 N.

The construction phase is going on but few vessels are painted but
baseline thickness measures to be taken. Awaiting valuable feedbacks
pl.

Thanks in advance,

Kumar.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp_UbmLrh-owzxWBk7cEm%2Bi3Yr0BYRMYge7Jn8b1HFN2Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...