Tuesday, November 29, 2016

[MW:25776] reg: Maximum interpass temperature in a WPS

Dear sir,

Refer to QW-406.8 of ASME sect. IX.

An increase in the maximum interpass temperature of more than 56degC from that achieved on the test coupon and record on the PQR.

In your PQR, interpass is 68degC.
So, max.interpass is 68+55 = 123degC.

Regards
Kurniatullah sirajudin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aa693611-06f8-4b0f-b7e5-54aee0b86999%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...