[MW:25730] WPS as per ASME SEc. IX

Dear Experts,

We have the following WPS as per ASME Sec. IX

Base metal - P5B + P8  (6" Sch 40 Pipe)
Welding process -  GTAW
Filler metal -  ER NiCr-3
Preheat temp - 180 degree C
PWHT - Nil
Trailing & backing gas -  Yes (Argon)

Can i use the above procedure for welding of ;

P5B group material fillet welding (seal welding of threaded joints) with ER NiCr-3 or ER NICrMo-3 GTAW process without PWHT 
Hardness test required for HAZ 235HV10.

your expert advice highly appreciated.

Thanks & Regards,
Manoj.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nE%3DtZ-gmMz2cg%3DzBTMjGpOTCxSxUQwT7jSRDWn3SkFXw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...