Wednesday, November 16, 2016

RE: [MW:25721] thickness on painted vessel

Prasard,
No you don't!
There are UT equipment's allowed take measurements...
without take paint..

regards,

Luciano Lucas




-----Mensagem original-----
De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Em nome de Prasad Rode
Enviada: terça-feira, 15 de Novembro de 2016 17:34
Para: Materials & Welding
Assunto: [MW:25707] thickness on painted vessel

Whts u r question is? Pls clarify.
To perform the Ut , u have to remove the paint.

Regards
Prasad Rode

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f105f84b-66bb-40de-af09-9548f40acd8c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

________________________________

O conteúdo desta mensagem de correio eletrónico e seus anexos é confidencial e de uso reservado.
Se não é o destinatário, não a guarde, não a reenvie a terceiros, nem faça qualquer uso da informação nela contida. Por favor, apague-a e informe de imediato o remetente. A Internet não garante a confidencialidade e a entrega correta de mensagens de correio eletrónico. A Galp não aceita responsabilidade por danos causados pela receção incorreta desta mensagem.
Apesar de esta mensagem ter sido verificada pelo nosso sistema de antivírus, não podemos garantir que não contenha vírus informáticos e não aceitamos qualquer responsabilidade por danos causados por vírus que possam estar contidos nesta mensagem.
Para informações sobre a Galp visite o nosso website em http://www.galp.com.

This e-mail and related attachments contain confidential and legally privileged information.
If you are not the intended recipient you must not keep it in your records or forward it to any third parties, nor use the information contained in it. Please delete it and notify by return Email. Internet email does not guarantee the confidentiality or the proper receipt of messages sent. Galp declines any liability for damages caused by improper receipt of this message.
Our own virus checking system has swept this e-mail and its attachments. However, we cannot guarantee that it is vírus-free and cannot take responsibility for any virus which may be present.
For further information about Galp please visit our website at http://www.galp.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B66AB34C6EFF99439E2C6A1EA2F79879282D29C0%40GEEXDAG02.oil.galpenergia.corp.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...