Monday, May 11, 2015

Re: [MW:23267] Flux Trade Name for SAW

1. Who will perform the classification test?
Flux & wire manufacturer
2. While reviewing the PQR, does the vendor need to submit Classification records?

The marking on the boxes / cans and the MTR is an evidence for classification
3. If a PQR is qualified with Flux Trade Name "X", can this PQR be used to support another WPS where Flux Trade Name "Y" is mentioned without classification? Please note, X & Y are from different manufacturer.

No

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Manas Ghosh ---11/05/2015 11:15:16---While qualifying a SAW Procedure as per ASME Sec IX, With respect to QW-404.9, the Flux Trade Name i

From: Manas Ghosh <m.k.ghosh1073@gmail.com>
To: materials-welding@googlegroups.com
Date: 11/05/2015 11:15
Subject: [MW:23265] Flux Trade Name for SAW
Sent by: materials-welding@googlegroups.com





While qualifying a SAW Procedure as per ASME Sec IX, With respect to QW-404.9, the Flux Trade Name is not an essential variable if the Flux Wire combination is Classified in ASME Sec II Part C (for A No 8, it is essential variable).

My queries are as follows
1. Who will perform the classification test?
2. While reviewing the PQR, does the vendor need to submit Classification records?
3. If a PQR is qualified with Flux Trade Name "X", can this PQR be used to support another WPS where Flux Trade Name "Y" is mentioned without classification? Please note, X & Y are from different manufacturer.

Please let me know your view. If you need further details, let me know.

Thanks and regards
Manas Ghosh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/6b0fedef-fe83-4f74-9e72-110cddda9bae%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...