Dear Experts,


Can you please give the reference below?


We have 2000 butt weld joints (2" * 6mm Thick) for RT in Power Boiler and the project time is so short and we proposed PAUT lieu of RT to our client.


Then client ask the reference from the code and we referred PW-11 & 52 as per ASME Sec. I but PW-11 is clearly mentioned that UT shall be carried out in circumferential weld of pipes and tubes more than 4" or thickness more than 13mm.


Can you please give the reference from ASME section to UT or PAUT lieu of RT for 6mm thickness of Pipe or Tube or power pipe.


Thanks & best regards,


M.Sudalai,

QA/QC Engineer.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BZM_eaZ_yLQt--N4vz7OOOGS01ZzzS0G0QMWVL39btN-X3-Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...