[MW:23031] Local PWHT of butt welds in piping

For long piping(Carbon steel, alloy steel), butt welding of large diameter(219mm OD TO 606mm OD, THK - 18.26mm to 42 mm )pipes is carried out. 
For PWHT of these butt welds, what are the parameters shall be considered for effective PWHT?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/123817e2-66c9-440c-9da6-21d6b616ce26%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...