Re: [MW:23022] DISCRPENCIES CHEMICAL COMPOSITION



Dear Eldho Isaac,

Note "e" is for ER5654/R5654 it means that value of 0.05 given for each element the beryllium should not exceed 0.0008 percent.
 
Note "k" is for R-A357.0 it means that the beryllium inclusion should be within given range of 0.04-0.07 percent. 

Regards,

Anosh 

From: Eldho Isaac <eldhoisaac4mech@gmail.com>
Sent: Sat, 23 May 2015 11:43:47
To: materials-welding@googlegroups.com
Subject: [MW:23016] DISCRPENCIES CHEMICAL COMPOSITION
Dear All,
With reference to attachment of SFA 5.10 Chemical Composition , can anyone please confirm the required values of Beryllium
As both the values given in the NOTEs " e" and " k"  are contradicting with each other.
Or is it a typographical error.
 
 
 
Regards,
 
 
Eldho Isaac

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJLt9FWUuYzhGbSA5Zia2v2xwheqbhEANDN0YoSS4DEBVefCmg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1432361627.S.3449255.14495.f4-234-162.1432374310.31233%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...