| MECHANICAL PROPERTIES (1) – As Required per AWS A5.4/A5.4M: 2006 | ||||
| Yield Strength (2) Tensile Strength Elongation Ferrite | ||||
| MPa (ksi) | MPa (ksi) | % | Number | |
| Requirements AWS E316-15, -16, -17 AWS E316L-15, -16, -17 | Not Specified | 520 (75) min. 490 (70) min. | 30 min. | Not Specified |
| Typical Performance (3)As-Welded 316/316L-15 316/316L-16 316/316L-17 | 470 (68) 425 - 450 (62 - 65) 470 (68) | 620 (90) 560 - 585 (81 - 85) 585 (85) | 38 40 - 54 45 | 4 - 12 8 - 13 13 |
| DEPOSIT COMPOSITION (1) – As Required per AWS A5.4/A5.4M: 2006 | |||||
| | |||||
| Requirements AWS E316L-15, -16, -17 | 0.04 max. C | 17.0 - 20.0 Cr | 11.0 - 14.0 Ni | 2.0 - 3.0 Mo | 0.5 - 2.5 Mn |
| Typical Performance (3)316/316L-15 316/316L-16 316/316L-17 | 0.02 0.03 - 0.04 0.03 | 18.6 - 19.3 18.7 - 19.2 19.1 - 19.7 | 12.0 - 12.4 11.4 - 12.1 11.6 - 12.7 | 2.2 - 2.6 2.2 - 2.4 2.1 - 2.4 | 0.7 0.7 - 0.9 0.8 - 1.0 |
| %Si %P %S %Cu | |||||
| Requirements AWS E316L-15, -16, -17 | 1.00 max. | 0.04 max. | 0.03 max. | 0.75 max. | |
| Typical Performance (3)316/316L-15 316/316L-16 316/316L-17 | 0.72 - 0.74 0.29 - 0.39 0.61 - 0.72 | 0.02 0.02 0.02 | 0.01 0.02 0.01 | 0.24 0.26 0.26 | |
Sent: Wednesday, May 13, 2015 11:37 AM
To: materials-welding@googlegroups.com
Subject: [MW:23275] Hey Dear Experts, what is the different between welding SS316 and 317?
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a85496b5-4203-4db2-a49f-03e6d9102140%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments