Re: [MW:23017] DISCRPENCIES CHEMICAL COMPOSITION

each one applies to different AWS classification, pl check the applicability indicated against each classification

On 23 May 2015 at 10:01, Eldho Isaac <eldhoisaac4mech@gmail.com> wrote:
Dear All,
With reference to attachment of SFA 5.10 Chemical Composition , can anyone please confirm the required values of Beryllium
As both the values given in the NOTEs " e" and " k"  are contradicting with each other.
Or is it a typographical error.
 
 
 
Regards,
 
 
Eldho Isaac


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubk46dpVe7Hvbsq-U8y-bquyupbb631EfUmHumpiFTWt6g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...