Dear Experts,
Do you have any data of lateral expansion at “0” deg [impact varying 120-140J] and “-40” deg [impact varying 60-90J] in mild steel for SAW process?
TnR
PT
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...