Dear Experts,

          I need to do tube to tubesheet mock up test, as per qw-193 the thickness of the tubesheet in the mockup test assembly shall be at least as thick as the production tubesheet, except it is not required to be thicker than 2 in. (50 mm),

Existing Design:
Tubesheet thickness is 85mm
Joint Detail: Double groove + expansion and groove with seal welding
Expansion area: full length leaving 3.2mm from back side.

Based on above said point tubesheet exceed 50mm thk there is no need to same as production coupon, so if i am taking 50mm thickness leaving 3.2mm from backside and remaining area expansion + welding it's correct way(expansion area is 47mm),but actual existing expansion area is 82mm, so I have to take 85mm to mock up test instead of 50mm or go with 50mm thickness with 47mm only expansion area which one is correct?
I attached 2d drawing of tube to tubesheet joint detail, Kindly clarify my doubt.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed0751db-4928-4db0-8431-20b4238e30ca%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...