thanks very much , i'll find it.
Vào 14:17:12 UTC+7 Thứ Ba, ngày 26 tháng 5 năm 2015, HAMID HAMIDI đã viết:
-- Vào 14:17:12 UTC+7 Thứ Ba, ngày 26 tháng 5 năm 2015, HAMID HAMIDI đã viết:
no problem, see aws d1.1 table 4.1 page 130. for more information see pre qualify wps .On Tuesday, May 26, 2015 9:19 AM, JERRY TUAN <jerr...@gmail.com> wrote:
Dear experts and seniors. If groove weld can cover for fillet weld, AWS D1.1 , can it cover for lap joint? Cause I read some where else in AWS D 1.1 that lap joint weld can be consider as fillet weld. Thanks all
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .75138ccf-9864-45ce-8198- 2977e5a9da56%40googlegroups. com
For more options, visit https://groups.google.com/d/optout .
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e47f13c6-d561-472d-abcb-a52debb95e71%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.