Dear All,
Let me know, what type of problem will come in back welding for large pore dia. pipe? As per company spec. the back welding is essential variable. If we want to do any inside weld have to make new WPS and get approval from company .
For ex. if any repair comes in root , in high thk. of weld for more than 25 mm , even easy to remove from inside why should remove from out side of pipe. what type of problem will come ?
In final pass the hardness will be higher i agree. any other ???????
Ramu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35754] interpration
Interpretation #: BPV IX-18-34 Record Number: 18-771 Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-