[MW:10057] Re: WPS & WPQR

Yes, you can do that untill you are fulfiiling the requirement of the
essential variables and supplementary variables (if applicables)for
welder.

Regards
Sandeep Kumar

On Feb 27, 1:08 pm, manoj john <manojac...@gmail.com> wrote:
> Dear members,
>
> I have one welder qualified  with one WPS.
>
> My question is can I employ that welder to weld in accordance with other
> WPS,  if the essential variables for welder performance are same.
>
> Thanks & Regards.
> Manoj.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...