MSMS,
 
NO, you cannot use it for qualifying any other wps, due to Corten is not listed in Sec II therefore you cannot use mechanical/metallurgical properties grouping criteria. 
 
Regards

Subject: RE: [MW:9929] Corten & carbon Steel weldability
Date: Fri, 18 Feb 2011 09:29:27 -0600
From: jhenning@deltak.com
To: materials-welding@googlegroups.com


See below

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, February 18, 2011 4:14 AM
To: materials-welding@googlegroups.com
Cc: muthusrinivasan muthuselvam
Subject: Re: [MW:9925] Corten & carbon Steel weldability

 

Hi,

   My request is : May Corten PQR qualify Carbon steels WPS NO and how we can approuv it from ASME IX ? See Sc IX, QW-424,  and previous post.

Regards

2011/2/18 muthusrinivasan muthuselvam <msms2k@gmail.com>

Dear Mr.Zakaria..

 

Corten is unspecified material as per ASME... you can say that as unassigned and preferred electrode is E 7018 W -made to order.

 

I hope this is for chimney or some container..

 

br,

 

msms

On Thu, Feb 17, 2011 at 9:14 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:

Hi all,

  I need to know the P number of corten steels, i have on PQR according ASME sect IX corten to corten, i need to use it to prepare WPS for Carbon steels but i have doute Corten is PN°1 or PN°3, serashing in internet : Equivalent Corten is ASTM SA 242, is it true?
--
GHRAB Zakaria

--

To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...