- Regarding the PWHT:-the thickness mentioned here,1 inch sch 80 and thickness up to 10 inch sch 40 CS SA106 Gr B would not call for any PWHT. Look up in B-31.3-Table 331.1.1.The minimum thickness for mandatory PWHT for carbon steels is 20mm (3/4") and above.
- If there is NACE sour service requirement then PWHT is usually mandatory.However MR-0175 Clause A-2.1.4 provided some waiver from PWHT for some C-Mn steels and allows them to be accepted in as welded condition. You may find the details in MR-0175.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of renga raja
Sent: Friday, February 25, 2011 7:39 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10013] piping modification after PWHT
--Dear Sir,
This is case for discussion.
Let us assume that piping for SA106 Gr B pipes are fabricated and radiographed and found OK. Then as per the requirement, next stage is Post weld heat treatment.
Size of the piping is vary between 1 inch sch 80 and extends upto 10 inch sch 40 CS SA106 Gr b NACE material.
Now if one completed the PWHT cycle and during mounting of the piping it seems that without doing the re cutting and rewelding it will not fit then, how we should go forward,
1) Can piping accepted by means of radiograph after rewelding and if RT OK then we can go ahead for final hydro test without PWHT.
2) One has to do again PWHT for that modified joint.
3) What is AEME verdict about that?
4) Whether UCS – 56 is mentioned about that, as it will seems that code mentioned about repair weld only and not for new weld after modification.
Pl have your views on above.
Regards,
Abhay
Ext 448
IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Regards,
Rengaraja.T
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments