[MW:10058] Difference between impact testing by ASTME23 and ASTM A370

Dear all, 

I have a procedure in which impact testing should have been done as per  ASTM A370 but it has been done as per ASTM E23

Is there any difference between the standard on how the impact tests are conducted? Would the difference effect the final values?
tha material was UNS 31803 pipe and was tested at minus 50 degree centigrade.

Thanks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...