Monday, February 28, 2011

[MW:10050] In-service welding qualification of SS pipe line

Dear all,
 
As per the scope of API 1104, It is restricted to be used for CS and LAS material.
 
Which code is to be followed for In-service welding qualification of SS pipe line.
 
 

Jaydeep Joshi | Welding Engineer, TDW India Limited

Plot No 16 | Phase –III | Alindra – Savli G.I.D.C | Taluka : Savli | Vadodara – 391 775

Board : +91-2667- 619900 | Fax : +91- 2667- 619501| Extension : 7845

E-Mail : jaydeep.joshi@tdwilliamson.com  | www.tdwilliamson.com

Cell: +91 9978959626

P    Before printing, Think about ENVIRONMENTAL responsibility

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...