Dear!
LTCS and CS differ by Heat treatment while manufacturing.
LTCS shall be treated to control their microstructure accordance with
varies temperature and some chemical composition changes between those
materials... LTCS material using for low temp. services...

Can anybody clear could we use this LTCS for high temp. services??

On 2/22/11, james gerald <gerry_tup@yahoo.com> wrote:
> LTCS is low temperature carbon steel which can be used at low temperatures
> according to the applicable specification.
>
> Yes is the answer to your query if impact tested at the required
> temperature.
>
>
> J.GERALD JAYAKUMAR
> 00919344954677
>
>
> --- On Tue, 2/22/11, ramu ramalingam <ramu.srivi@gmail.com> wrote:
>
>
> From: ramu ramalingam <ramu.srivi@gmail.com>
> Subject: Re: [MW:9972] LTCS
> To: materials-welding@googlegroups.com
> Date: Tuesday, February 22, 2011, 7:37 AM
>
>
> what is the difference between CS & LTCS material.some time material heat
> numbers were both in one manufacturing and chemical and mechanical both are
> same in both materials.but one had impacted.Is it ok? Material can be used
> in production?
> Ramu
>
>
> On Thu, Jan 27, 2011 at 3:23 PM, Karthik <karthik6684@yahoo.com> wrote:
>
>
>
>
>
> Low Temperature Carbon Steel (LTCS)..This material used for Low temperature
> application on pressure vessels etc.,
>
>
> Thanks & Regards,
>
>
>
> (Karthik)
>
>
>
> Karthikeyan.S
> QA/QC Manager
> Getabec Energy Co.,Ltd.
> 379,Moo6,Soi8,Nikhomphatana,
> Rayong-21180,
> Thailand.
> Phone: 0066 38 897035-8 (Off)
> Fax: 0066 38 897034
> Hand Phone: 0066 892512282
>
> --- On Thu, 1/27/11, Pardeep <fab_qc@isgec.com> wrote:
>
>
> From: Pardeep <fab_qc@isgec.com>
> Subject: [MW:9522] LTCS
>
> To: materials-welding@googlegroups.com
> Date: Thursday, January 27, 2011, 3:55 PM
>
>
>
>
>
>
>
> Can any body tell me what is LTCS and its full form.
>
>  (Before Printing, Think about the environment, every 3000 A4 paper costs 1
> tree. Please DO NOT print unless you really need it. This will preserve
> trees on planet earth.)
>
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of muthu barathi
> Sent: Thursday, January 27, 2011 1:35 PM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:9517] CS in place of LTCS
>
> hi
>
> If cooling water , then the CS pipe tested with impact and the
> temperature should be more than your fluid temperature . if the fluid
> temperature is (-))10 deg C then your base metal should be at least (-)
> 20 deg C. in this way your CS is there then you may replace or you have
> to go for LTCS.
>
>
> On Thu, 27 Jan 2011 12:39:26 +0530 wrote
>>Can we replace LTCS with CS if temperature minimum expexted is
>
> -20DegC,process fluid;Coolwing water???
>
>
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-
> welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg at http://materials-
> welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
>
>
> Dear Sir,
>
>
>
>
>
> Thanking You,
>
> Honesty is the best Policy
>
> With Warm Regards,
>
> Muthu Barathi P
> Mobile No:00962788269821 (Jordan)
> 00962775401951
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...