dear
no,but it is recommended the filler be low H2 ELECTRODE(7018,7018-1,etc.) 
H.KASHKOUSHA



From: GRH <grhashemi2010@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Mon, February 28, 2011 9:40:34 AM
Subject: [MW:10051] Welding filler metal for H2+HCBN TRACES medium ( hydrocracker unit)

Dear Mr./Miss./Mrs.
The air cooler in HYDROCRACKER unit (oil refining plant)have the below
specifications,Please guide me about the welding procedure ,filler
metal and any requirements in conform to service.
design pressure:55.3 bar/f.v
design temperature:171 celsius
fluid circulated: H2+HCBN TRACES
X-ray examination:spot
PWHT:yes (Max. weld hardness;200 brinnel)
Materials:SA-516Gr.60 , SA-105 , SA-234WPB
Headers Thk.:30 mm.
This air cooler is in first steps of construction and only the main
drawing is available.the old equipment shall be replaced by the new.
Any supplementary date or detail is out of availability.
in API 661 some requirements like as low hydrogen content , ... is
mentioned, but it is possible the medium/service make the more
restriction that is not mentioned or detailed in this standard,
Is there any requirement for filler metal or welding process in
relation to medium (H2+HCBN TRACES) or service (hydrocracking)?
With best regards.
GRH
28.02.2011

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...