Sunday, February 27, 2011

Re: [MW:10039] WPS & WPQR

dear
yes you can,in condition  within the same
code requirements
H.KASHKOUSHA



From: manoj john <manojacgnr@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, February 27, 2011 10:08:39 AM
Subject: [MW:10037] WPS & WPQR

Dear members,
 
I have one welder qualified  with one WPS.
 
My question is can I employ that welder to weld in accordance with other WPS,  if the essential variables for welder performance are same.
 
Thanks & Regards.
Manoj.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...