First You have to select the suitable Electrode/Filler Rod from your experience or based on Technical Literature. The suitable electrode for welding IS2062 Gr.A to SS 410 is either E309L or Nickel based consumables like ENiCrMo3/E NiCrFe2/3. Then check for the A.No in QW-442 as A8 for E309L & A4X for Nickel based electrodes Then based on the SFA number(obtained from Sec.IIC) for the particular electrode, F number can be determined like F5 for E309L etc...
J.GERALD JAYAKUMAR 00919344954677
--- On Tue, 2/22/11, puneet takiar <puneet1takiar@yahoo.com> wrote: From: puneet takiar <puneet1takiar@yahoo.com> Subject: Re: [MW:9967] P1 no Range To: materials-welding@googlegroups.com Date: Tuesday, February 22, 2011, 5:42 AM
Dear Colleagues, Can anybody help me in describing method to select Electrode for welding SS to M.S ( IS2062 Gr.A to SS 410). As per sextion IX table QW 442, A no. will be 6 ( is it ok) and how i can find F no. w.r.t A no. whether there is any coorelation of A no. with F no. or not? OR their function is different w.r.to each other. please help. If the F no. is to be selected by experience then how the table of F no. in QW 432 is helpful. Warm regards, puneet takiar
From: jaya anil <nethalaanil@gmail.com> To: materials-welding@googlegroups.com Sent: Mon, 31 January, 2011 6:18:40 PM Subject: Re: [MW:9601] P1 no Range Dear Puneet, IS 2062 Gr A, is unlisted , but max. properties were equalent to P1. but while preparing WPS/PQR use Material Spec as IS 2062 GrA . SS 410 is Martensitic Steels, its P No is 6
On Sun, Jan 30, 2011 at 8:04 PM, puneet takiar <puneet1takiar@yahoo.com> wrote: Hello! Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table. Regards, puneet takiar
From: Karthik <karthik6684@yahoo.com> To: materials-welding@googlegroups.com Sent: Fri, 7 January, 2011 1:46:08 PM Subject: Re: [MW:0] P1 no Range Hi, Please refer QW423 also QW 350 for essential variables.
Thanks & Regards,
(Karthik)
Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
--- On Fri, 1/7/11, sn vl <weldinspn@gmail.com> wrote: From: sn vl <weldinspn@gmail.com> Subject: [MW:9122] P1 no Range To: "Materials & Welding" <materials-welding@googlegroups.com> Date: Friday, January 7, 2011, 2:43 PM
Hi.. How to find in ASME sec IX P no to Pno qualification range. Eg : If a welder qualified for P1to P1 what is the Range qualified As per Sec IX. Where is given in CODE. Regards SN. -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+ unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments