Re: [MW:9986] Nitrogen Purging for SB 409 Alloy 800H



On Wed, Feb 23, 2011 at 5:06 PM, P.Rao <vasantharao2009@rediffmail.com> wrote:

Dear All,

Can i use nitrogen Purging for GTAW Welding of subject material.

Are there any consumables available with Flux cored type?

I have a requirement to weld subject material from single side with ERNiCr-3 wire + ENiCrFe-2 electrodes. Single side only accessible.

Pl. provide your values inputs.

P.Rao

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...