Hi Firman,
See the attached article for your reference on PCM.This formula is a Japanese equivalent of IIW Carbon Equivalent formula. I would think this formula works better for HSLA or other micro alloyed steels, or typically for pipeline steels.
This article explains the pros and cons of all 3 popular formula for calculation of preheating temperature.
Feel free ask any queries, if you wish to.
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario, Canada.
Email-pgoswami@sympatico.ca,
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Firman Bhaktiwinaya
Sent: Sunday, January 30, 2011 10:24 PM
To: materials-welding@googlegroups.com
Subject: [MW:9562] PCM (Parameter Crack Measurement)
Dear All,
Please suggest me any information about PCM (Parameter Crack Measurement).
Regards,
Firman
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com