Monday, July 26, 2010

[MW:6127] inconell 625 weld cladding on AISI 4130 material


 Dear Team members,
 
It is required to qualify Nickell Alloy 625 overlay (10% FE max) on AISI 4130 at 1/8" minimum finished overlay deposited thickness.
Have anybody ever been faced with this before to share the experiance?
 
thanks.
Martin.