I HAVE FEW QUESTIONS TO ASK BEFORE COMMENTING ANYTHING ON THIS.
1. WHAT IS THE INCLUDED ANGLE OF THE GROOVE?
2. WHAT IS THE ESO YOU ARE TAKING AND WHAT IS RECOMMENDED BY
MANUFACTURER.
3. WHAT ARE THE WELDING PARAMETERS
4. AT WHAT LOCATION, WITHIN THE GROOVE, YOU ARE GETTING LOF/
POROSITIES?
5. BEAD DEPOSITION IS STRINGER OR WELDER IS EMPLOYING WEAVING
TECHNIQUE?

PLEASE CLARIFY.

SANJAY JAIN


On Sep 19, 10:42 pm, "PREM SHANKARDUTT NAUTIYAL"
<prem_nauti...@rediffmail.com> wrote:
>   
> Dear Friends
>
> We are presently using FCAW process(E71T-1) for welding SA516Gr.70 material in 3G and 1G. The joint calls for 100% RT and UT. The thickness is 70mm with double V.
> But everytime we get repair in the weld like slag, LOF,porosities..
>
> So my basic question is can FCAW be used to weld RT and UT joints??
> If yes what is the correct procedure / precautions to be followed..
>
> Regards
>
> Prem Nautiyal
>
> PREM S NAUTIYAL
> CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...