Dear Shailesh,
 
There is no thumb rule for the formation of HAZ. This largely depends on welding procedure, equipment used, various consumables, electrical parameters, operators skill and the uncertainities contributed by them. Normally one should expect minimum HAZ as is it not a desirable phenomena in any welding process.
 
N. Kalyan.
ELCA Laboratories.
 
 
----- Original Message -----
Sent: Monday, October 27, 2008 6:53 PM
Subject: [MW:1247] Re: HAZ

DEAR SACHIN,
 
LET ME MAKE MY QUESTION CLEAR TO YOU. FROM WELD JOINT END HOW MUCH IS THE WIDTH OF HAZ.
 
REGARDS,
 
SHAILESH

--- On Mon, 10/27/08, sachin sankhe <sachin.sankhe@rediffmail.com> wrote:
From: sachin sankhe <sachin.sankhe@rediffmail.com>
Subject: [MW:1246] Re: HAZ
To: materials-welding@googlegroups.com
Date: Monday, October 27, 2008, 5:34 PM


Hi Shailesh
Your question is not clear

Regards
Sachin

On Sat, 25 Oct 2008 shailesh dave wrote :
>DEAR MEMBERS,
>
>WOULD YOU PLEASE TELL ME WHAT COULD ME THE THUMB RULE FOR HEAT AFFECTD ZONE DURING WELDING.
>
>REGARDS,
>
>S.N.DAVE
>I/C QA/QC DAS ISLAND UAE
>
>
>
>>



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...

ICL

Pages

Contributors

Blog Archive