[MW:1245] Re: Which WPS can be used

 If your production weld is undergoing PWHT than u have to use with PWHT WPS otherwise without PWHT. Base material Heat treatment condition before welding is not essential & also with base metal heat treatment condition u cannot decide WPS - PWHT requirement.

On Sun, Oct 26, 2008 at 12:38 PM, <kataiah@bilfal.com> wrote:

Dear Frinds ,

I have a requirement to weld  Stress relievedCS  plate # normal CS Plate.

Which WPS can is use to weld such combination ( i mean a WPS with PWHT or with out PWHT).

ASME is refering anywhere which type to be used?

What is the logic to use perticular type?.

Regards

P.K.
Bilfal Industries.

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...